供应雨停回填宝

产品特点: ★ 进口主原料,性能卓越 ★ 轻质环保,无需做抹面层可直接贴砖 ★ 不收缩、不下沉、抗压性能强 ★ 耐候性好,与主体同寿

访问量:

产品简介 Product Introduction

雨停回填宝回填找平材料采用高分子聚合物、砂浆稳定剂精制而成,现场加水和水泥经专用搅拌机混合而成,是一种含有大量封闭气孔的新型轻质材料,具有质量轻、强度高、不收缩、抗开裂、阻水耐久的优异特性,解决卫浴间沉箱积水、地面找平、减轻建筑负重,达到环保节能、省工、省料的理想效果。 

 

The YUTING backfill treasure of macromolecule polymer, slurry stabilizer refined but become, special field water and cement mixer, which is a mixture is a new type of lightweight materials containing a large number of closed pores, with light mass, high strength, no shrinkage, crack resistance, water resistance excellent properties of endurance, solving caisson water between wei yu, ground leveling, reduce building load, achieve environmental protection and energy saving, of the province, the ideal effect.

 

性能特点 Product Feature

·抗压强度高,现场整体浇注,内外一致,不收缩、不开裂、抗压强度可达1mp以上。 

·流动效果好,搅拌好的浆料注入基有良好的流动性,有效填封管道周边缝隙,封堵沉箱防水层施工无法做到位的死角。 

·阻水耐久,吸水率低,表面明显的荷叶效果,气孔独立不串通,有效阻隔水的流通,主要成分为水泥,与主体结构同寿命。 

? high compressive strength, overall pouring on site, internal and external consistency, no shrinkage, no cracking, compressive strength can reach above 1mp.

? good flow effect, good flow of the slurry injected into the base surface, effective sealing of the surrounding cracks of the pipe, sealing off the blind Angle of the caisson waterproof layer, which cannot be achieved.

 

? durable water resistance, low water absorption rate, obvious lotus leaf effect on the surface, independent and non-collusion pores, effectively blocking the flow of water, the main composition is cement, with the same life as the main structure.

适用范围 Range of Application

·卫浴间沉箱回填、房间客厅地面找平、屋面防水层保护隔热等施工。

? refilling of caisson between bathroom and bathroom, leveling of the living room floor, roof waterproof layer protection and heat insulation, etc.

 

施工程序与方法 Construction Procedure

·在搅拌容器内倒入40公斤水,开动搅拌机到高速挡,倒入一袋A料搅拌5分钟,泡沫到达标准位置,调到低速挡运行,缓缓加入50公斤水泥,再加入B料充分搅拌5分钟至均匀的膏糊状。 

·打开阀门把浆料注入沉箱或基面,流到指定位置后关闭阀门,用刮板稍稍刮平待其表干。 

? pour 40kg of water into the mixing container, start the mixer to high speed, add one bag of material A and B, and stir for 3 minutes. When the foam reaches the standard position, adjust to low speed, slowly add 50kg of cement, and stir well for 3-5 minutes until the paste is smooth and smooth.

 

? open the valve and inject the slurry into the caisson or base surface, flow to the designated position and close the valve.

     注意事项 Notice

·施工前请仔细阅读包装说明,按规定流程操作。 

·加入32.5R与42.5R水泥干固时间和强度会有所差异,如工期较紧建议使用42.5R水泥施工。

·浇注完工未完全干固禁止踩踏,以免影响施工效果。

·施工完成后立即清洗干净机器和阀门,以免水泥结块堵塞阀门。

·严禁开机后伸手入机器桶内,以防发生意外。

? please read the packing instructions carefully before construction and operate according to the specified procedures.

? adding 32.5r and 42.5r will have differences in drying time and strength. If the construction period is tight, 42.5r cement is recommended for construction.

? no trampling is allowed if the pouring is not completely dry, so as not to affect the construction effect.

? clean the machine and valve immediately after construction to avoid clogging the valve with cement.

? it is strictly forbidden to reach into the machine barrel after starting up, in case of accident.

贮存方法 Preservation Method

本产品放置于阴凉干燥处,勿让儿童触及,保质期为12个月。

 

This product is placed in a cool and dry place, not to be touched by children, with a shelf life of 12 months.

 

参考用量 Dosage

参考用量Dosage of reference

每桶内装6组A、B料,一组配50公斤水泥,每桶约浇注1m3左右。

 

Each barrel is filled with 6 sets of materials A and B, and one group is equipped with 50 kilograms of cement, about 1m cubed per barrel is poured.